Abstract
For decades it has been a clinically accepted requirement, in case of salivary contamination, to re-etch conditioned enamel and dentin to proceed with the adhesive technique. Only a few reports have been so far dealing with the potential of one-bottle adhesive system to bond even when applied after salivary contamination and without re-etching. The purpose of this study was to evaluate the influence of the salivary contamination on the shear bond strength of dentin. The results were as follows: 1. In group II, in which saliva contamination and washing occurred before applying of Prime & Bond NT showed high shear bond strength as in control group. In Group III and IV, in which the cured adhesive was contaminated with saliva, showed significantly lower mean bond strength, 2. Relating long resin tags of 70~120μm were observed in samples of all groups under SEM. We could observed hybrid layer, resin tag and many lateral branches in every group. And there were no differences between groups.
Key Words: Saliva contamination, One bottle adhesive system, Re-etchinng


ABOUT
BROWSE ARTICLES
EDITORIAL POLICY
FOR CONTRIBUTORS
Editorial Office
Seoul National University, Dental Hospital, B1-166 101, Daehak-ro, Jongno-gu, Seoul 03080, Republic of Korea
Tel: +82-70-4145-8875    Fax: +82-2-745-8875    E-mail: info@kapd.org                

Copyright © 2024 by Korean Academy of Pediatric Dentistry.

Developed in M2PI

Close layer
prev next